ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications has approved a standard covering a test chamber used by transportation departments and similar agencies throughout the world to specify and test the dry speed of waterborne pavement marking paints at elevated relative humidity. The new standard, ASTM D7539 , Practice for Using a Test Chamber for Humidity…, ASTM Committee D01 Next Meeting:, Jan. 30-Feb 1, 2011, January Committee Week, Baltimore, Md., Technical Contact:, Donald Schall, Dow Chemical Co., Spring House, Pa., Phone: 215-641-7163; dschall@dow.com, ASTM Staff Contact:, Jeffrey Adkins, Phone: 610-832-9738; jadkins@astm.org, ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #8675/Sept2010
-
Trona, or sodium sesquicarbonate, is a fine mineral powder that has proven to be effective at removing acid gases from air emissions. While trona can be a useful component of air pollution control systems, it can be difficult to handle, particularly when moisture is present. A proposed new ASTM standard will present a repeatable, precise and accurate test method for analyzing moisture levels in…, ASTM Committee E01 Next Meeting:, Nov. 14-17, November Committee Week, San Antonio, Texas, Technical Contact: J, ames D. Phillip, Solvay Chemicals Inc, Green River, Wyo., Phone: 307-872-6519; jim.phillip@solvay.com, ASTM Staff Contact:, Thomas O'Toole, Phone: 610-832-9739; totoole@astm.org, ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #8608
-
ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications, has approved two new standards that cover architectural coating touch-up properties and ink stainblocking of paint systems. Both new standards are under the jurisdiction of Subcommittee D01.42 on Architectural Coatings., Touch-Up Properties, When a home is being constructed, paints are subjected to a wide variety of drying conditions, which can lead to differences in appearance between the original coat and subsequent touch-up areas after the paint has fully cured. A new standard, ASTM D7489 , Practice for Evaluating Touch-Up Properties of Architectural Coatings Under Various Environmental Conditions, covers variations in color,…, Ink Stainblocking, Paint companies and raw material suppliers will be able to use a new ASTM standard to assess the capability of architectural coatings for blocking ink stains from bleeding through to a topcoat. The standard, ASTM D7514 , Test Method for Evaluating Ink Stainblocking of Architectural Paint Systems by Visual Assessment, represents a compilation and synthesis of methods that are currently being used…
-
Test Method Covers Inductively Coupled Plasma Atomic Emission Spectrometry, A new ASTM International standard will help users properly prepare and analyze various nickel-based alloy samples by inductively coupled plasma emission spectrometry. The standard, ASTM E2594 , Test Method for Analysis of Nickel Alloys by Inductively Coupled Plasma Atomic Emission Spectrometry (Performance-Based Method), will assist users in preparing sample and calibration solutions and with…
-
Traffic paint plays an important role in maintaining the safety of roads. Subcommittee D01.44 on Traffic Coatings, part of ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications, is currently working on two proposed new standards covering the sampling of waterborne traffic paint and glass bead gradation measurement., WATERBORNE TRAFFIC PAINT, Ensuring that traffic paint taken from the field is tested properly in laboratories is a concern of paint suppliers as well as private testing laboratories, Department of Transportation labs, DOT striping crews and striping contractors. A proposed new ASTM standard, ASTM WK22312 , Practice for Drum and Tote Sampling of Waterborne Traffic Paint, addresses laboratory sampling issues. According to…, GRADATION OF GLASS BEADS, Glass beads added to traffic paint during manufacturing are necessary to ensure paint retroreflectivity, especially at night. A proposed new standard, ASTM WK23758 , Test Method for Measuring Gradation of Glass Beads Using a Flowing Stream Digital Image Analyzer, will be useful in the production and quality control of glass beads. “Digital camera technology combined with high speed computers has…
-
More effective quality testing of the synthetic, hollow filaments that are often used in the manufacture of lower cost paintbrushes is the purpose of a new standard approved by ASTM International Committee D01 on Paint and Related Coatings, Materials and Applications. The new standard, ASTM D7233 , Test Method for Testing Fracture of Level Paintbrush Filaments, was developed by Subcommittee D01.…
-
The wettability of a particular solid coating, substrate or pigment on a surface is a key to its effectiveness, as wetting is important to adhesion as well as to the prevention of surface defects such as craters, dewetting and crawling. A new ASTM International standard uses contact angle measurements to determine the wettability of coatings. The new standard, D7490 , Test Method for Measurement…
-
Providing practical advice on the use of infrared thermometers is the purpose of a proposed new ASTM International standard. Infrared thermometry is used in a variety of measurement applications, including heating, ventilating and air conditioning, building inspection, industrial and manufacturing, automotive and food service equipment. The proposed new standard, ASTM WK21204 , Guide for the…
-
Advancing gas analysis technology is leading to the development of a proposed new ASTM International standard, WK22331 , Test Method for Simultaneous Determination of Oxygen, Nitrogen and Hydrogen in Titanium and Titanium Alloys by the Inert Gas Fusion Technique. Analyzers are now available that can simultaneously test titanium and titanium alloys for oxygen, nitrogen and hydrogen. This…
-
By necessity, paint used for roadway applications needs to dry quickly. Some multi-component traffic paints cure in less than 10 minutes, some much faster. Because of this speed of curing, these traffic paints and other types of fast-cure (less than 10 minutes) multi-component paints cannot be tested for volatile content using procedures outlined in the ASTM International standard typically used…