John Kohler, technical specialist - elastomers, FCA US LLC (Fiat Chrysler Automobiles), Auburn Hills, Mich., has been named chairman of ASTM International Committee F09 on Tires . Formed in 1971, F09 has over 85 members, and includes 7 technical subcommittees that oversee more 38 standards related to tire characteristics and performance, research, and vehicular testing. Kohler has been a member…, Media Inquiries:, Dan Bergels, tel +1.610.832.9602; dbergels@astm.org Release #10056
-
A new ASTM International standard will help concrete manufacturers that use steel wires in their products. The standard was inspired by the assessment of concrete railroad ties that used indented prestressing wires which had possible bond-related cracking problems, according to ASTM member Robert Peterman, the Mark H. and Margaret H. Hulings Chair in Engineering, Kansas State University. The new…, ASTM Committee A01 on Steel, Stainless Steel and Related Alloys Next Meeting:, May 17-20, May committee week, St. Louis, Mo., Media Inquiries:, Nathan Osburn, tel +1.610.832.9603; nosburn@astm.org, Technical Contact:, Christopher Reeve, Insteel Wire Products, Gallatin, Tenn., tel +1.615.451.6330, ext. 2762; creeve@insteel.com, ASTM Staff Contact, : Kevin Shanahan, tel +1.610.832.9737; kshanahan@astm.org Release #10015
-
The expected discontinuance in manufacturing a standard-reference test tire will lead to changes to an ASTM International standard ( E1136 , Specification for P195/75R14 Radial Standard Reference Test Tire). Users of this specification are invited to join an ASTM task group that is working to manage this transition. The tire has been used extensively since its introduction in the late 1980s.…, ASTM Committee F09 on Tires Next Meeting:, Oct. 13-14, 2015, MAPS Air Museum, North Canton, Ohio, Media Inquiries:, Nathan Osburn, tel +1.610.832.9603; nosburn@astm.org, Technical Contact:, Angela Wolynski, Michelin North America, tel +1.864.422.4985; angela.wolynski@us.michelin.com, ASTM Staff Contact:, Julia Lively, tel +1.610.832.9681; jlively@astm.org Release #9880
-
A new ASTM International standard supports corrosion protection for steel reinforcing bars galvanized by zinc or zinc-alloy coatings for protection from corrosion. The standard ( A1094/A1094M , Specification for Continuous Hot-Dip Galvanized Steel Bars for Concrete Reinforcement) provides a high-performance, low cost option for building and protecting concrete structures. ASTM member Gary…, ASTM Committee A01 on Steel, Stainless Steel and Related Alloys Next Meeting, : Nov. 16-19, 2015, November Committee Week, Tampa, Fla, Media Inquiries:, Nathan Osburn, tel +1.610.832.9603; nosburn@astm.org, Technical Contact:, Gary W. Dallin, GalvInfo Center, Burlington, Ontario, Canada, tel +1.905-315-7443; gdallin@cogeco.ca , ASTM Staff Contact:, Kevin Shanahan, tel +1.610.832.9737; kshanahan@astm.org Release #9832 ###
-
A new ASTM standard tests the potential of a pressurized aerosol product to be accidentally inhaled and aspirated (drawn into the respiratory tract of those near the spraying). The standard ( D7952 , Test Method for Measuring Aspiration Potential of Aerosol Products) specifically tests aspiration potential by determining spray pattern and aerosol deposition rates. Aspiration can potentially cause…, STM Committee D01 on Paint and Related Coatings, Materials and Applications Next Meeting:, June 21-23, 2015, Ft. Lauderdale, Fla., Media Inquiries:, Nathan Osburn, tel +1.610.832.9603; nosburn@astm.org, Technical Contact:, Woodhall Stopford, Duke University Medical Center, Durham, N.C., tel +1.919.732.7442; woodhall.stopford@duke.edu, ASTM Staff Contact:, Jeffrey Adkins, tel +1.610.832.9738; jadkins@astm.org Release #9835 ###
-
Pigment manufacturers use the loss on ignition test to determine water of hydration or crystallized water. While loss on ignition is a frequently used test, its methodology is embedded within other standards and varies from one to another. Now, a proposed new standard, ASTM WK46877, Test Method for Pigment Loss on Ignition, will provide definitive instructions for conducting this common test. “…, ASTM Committee D01 Next Meeting:, Jan. 25-27, 2015, January Committee Week, New Orleans, La., Technical Contact:, Steven Brunner, WPC Technologies, Milwaukee, Wis., Phone: 414-225-2415; sbrunner@wpctech.com, ASTM Staff Contact:, Jeffrey Adkins, Phone: 610-832-9738; jadkins@astm.org, ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #9682
-
Infrastructure projects rely on reinforced concrete as a principal construction material. Each year, more than $1.3 trillion is spent constructing new infrastructure or repairing/replacing old infrastructure for energy, water, communications and transportation systems. A proposed ASTM International standard will cover the protection of zinc-coated steel bars used for concrete reinforcement in…, ASTM Committee A01 Next Meeting:, Nov. 10-13, 2014, November Committee Week, New Orleans, La., Technical Contact:, Gary W. Dallin, GalvInfo Center, Burlington, Ontario, Canada, Phone: 905-315-7443; gdallin@cogeco.ca, ASTM Staff Contact:, Kevin Shanahan, Phone: 610-832-9737; kshanahan@astm.org, ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #9658
-
The steel bases of power transmission poles are a critical but often unnoticed component of electrical infrastructure. Proper performance of such bases helps ensure uninterrupted power to homes, businesses, schools and any other venue using electrical power. A new ASTM International standard, ASTM A1090/A1090M , Specification for Forged Rings and Hollows Produced from Steels with Atmospheric…, ASTM Committee A01 Next Meeting:, Nov. 10-13, 2014, November Committee Week, New Orleans, La., Technical Contact:, Patrick Nowak, Scot Forge, Clinton, Wis., Phone: 608-676-2288; pnowak@scotforge.com , ASTM Staff Contact:, Kevin Shanahan, Phone: 610-832-9737; kshanahan@astm.org , ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #9652
-
A proposed new ASTM International standard is emerging from research being conducted at the U.S. Bureau of Reclamation to identify and investigate coatings that will prevent the settlement and attachment of erosion-causing invasive species such as zebra and quagga mussels inside water and wastewater pipelines. The proposed standard, ASTM WK45207 , Test Method for Erosion of Coatings by Flowing…, ASTM Committee D01 Next Meeting:, June 22-24, 2014, in conjunction with ASTM International Committee D02 on Petroleum Products, Liquid Fuels and Lubricants meeting, Indianapolis, Ind., Technical Contact:, Daniel Libby, Chase Corp., Westwood, Mass., Phone: 781-332-0782; dlibby@chasecorp.com, ASTM Staff Contact:, Jeffrey Adkins, Phone: 610-832-9738; jadkins@astm.org , ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #9645
-
An ASTM subcommittee is developing a proposed standard to test the slip coefficient properties of coatings used in slip-critical bolted connections. The test is based on an appendix in the “Specification for Structural Joints Using High-Strength Bolts,” published by the Research Council on Structural Connections. The proposed ASTM standard will expand on the Research Council standard by…, ASTM Committee D01 Next Meeting:, June 22-24, 2014, Indianapolis, Ind., Technical Contact:, Bill Corbett, KTA-Tator Inc., Pittsburgh, Pa., Phone: 412-788-1300, ext. 223; bcorbett@kta.com , ASTM Staff Contact:, Jeffrey Adkins, Phone: 610-832-9738; jadkins@astm.org , ASTM PR Contact:, Barbara Schindler, Phone: 610-832-9603; bschindl@astm.org Release #9638